Zirconium Grade 702 Technical Report
Chemical Composition |
Element |
Grades R60702 |
Zirconium + hafnium, min |
99.2 |
Hafnium, max |
4.5 |
Iron + chromium, |
0.2max |
Tin |
…. |
Hydrogen, max |
0.005 |
Nitrogen, max |
0.025 |
Carbon, max |
0.05 |
Niobium |
…. |
Oxygen, max |
0.16 |
|
|
Mechanical Properties:
|
Zirconium and Zirconium Alloy Strip, Sheet, and Plate |
Tensile Requirements |
R60702 |
Tensile strength, min, ksi [MPa] |
55 [380] |
Yield strength, min, ksi [MPa] |
30 [205] |
Tensile strength, max, ksi [MPa] |
... |
Yield strength, max, ksi [MPa] |
|
Elongation in 2 in. or 50 mm, min, %A |
16 |
Bend test radiusB |
5T |
|
|
Zirconium and Zirconium Alloy Bar and Wire |
Tensile Requirements |
R60702 |
Tensile Strength, min, ksi (MPa) |
55 (380) |
Yield Strength, min, ksi (MPa) |
30 (205) |
Elongation in 2 in. or 50 mm min, % |
... |
|
|
|
|
|
|
Find Better Metal for Better Future |
|
|
|
|
 |
|